scm440 硬度 hrc的相關文章
scm440 硬度 hrc的相關金屬表面處理公司資訊
scm440 硬度 hrc的相關商品
Manufacturing procedures of a 17-4 PH part - Metal and Metallurgy engineering - Eng-Tips
瀏覽:1366
日期:2024-11-08
Hi friends, I have a part which it's material is 17-4PH ss and H1025 condition is requested. I know after H1025 the hardness might up to 38HRc. So I have to lea ... I presumed that the only finishing was machining. If you are going to bend, form, weld, sw...看更多